Two Materials - One Ceramic
Triceram® is a time tested German porcelain system for both Titanium & Zirconia. Triceram® bonder produces a bond strength which far exceeds the required standard. This eliminates the problem of inadequate bond strength which has been associated with some titanium ceramics in the past. Various universities in Germany and abroad have carried out extensive scientific tests which verify both the excellent bond strength as well as high fracture load of the Triceram® porcelain system.

In addition to being exceptionally strong, Triceram® boasts a natural shade effect with remarkable luminescence. Because Triceram® is a synthetic bonding ceramic, it has the advantage of producing different shade effects. Due to the chameleon effect of Triceram®, the light flows through the restoration enabling the shades of the restoration and residual dentition to blend. Your patients will enjoy a long lasting restoration that is not only strong, but exceptionally beautiful.

Fracture loads and respective Weibull parameters of veneered crowns
(SD: standard deviation;* : significantly different to Degudent U (p<0.05)).2
Core Material Ceramic Load at fracture (N) mean (±SD) Weibull Modulus m Weibull Strength
σ 63.21% (N)
Zirconia Y-TZP IPS e.max 818.0 (±127.2)* 7.4 872.2
Cerabien ZR 836.0 (±117.3)* 8.3 885.9
Lava Ceram 852.3 (±131.9) 7.5 907.7
Zirox 855.2 (±145.8) 7.0 914.1
Rondo Zirconia 849.9 (±119.2) 8.3 900.1
VM9 935.2 (±186.3) 5.9 1009.4
Triceram 930.5 (±145.8) 7.5 990.4
Titanium Triceram 898.6 (±105.7) 10.0 943.4
Vita Ti 762.9 (±105.6)* 8.5 806.8
Degudent U VM13 990.0 (±161.3) 7.1 1057.9

ORIGIN Dental CAD CAM Triceram

  • University of Freiburg,Germany,Prof.Dr Kappert H.F.:Bruchfestigkeit und Frakturverhalten von DCS-gefrästen Frontzahnkronen nach Verblendung mit Vitadur Dund
    Triceram ,ZWR,2001:134-139,(DC-Zirkon‚)
  • University of Nantes,France,Praud C.:Dissertation:Rapport de la Céramique Triceram à la réalisation de prothèses céramo-métalliques sur Titane:1999
  • University of Munich,Germany,Bader R.-D.,Aschl I.,Rammelsberg P.Pospiech P.:IADR Abstracts 1021: Improved bond strength of low fusing ceramics to titanium: 2000
  • Dental Materials Journal 26(6), 766-772, 2007: Effect of Thermal Misfit between Different Veneering Ceramics and Zirconia Frameworks on in vitro Fracture Load of Single Crowns